Polyolefin catalysts and polyolefin resin

Focus On Catalysts

Devoted To Polyolefin

PE Catalyst


***Polymerization condition:2L reactor,1L hexane as solvent, 85℃,2hour,H2/C2=0.28/0.75(MPa)

Previous: None
Next: None
Customized Solution
PE Catalyst
Quality Commitment
Proprietary Technology and Advantage
Customers
Products
PP Catalyst
PE polymer from Lihe Catalyst
PP Polymer from Lihe catalyst